摘要 |
<p>PROBLEM TO BE SOLVED: To provide a fiber reinforced thermoplastics joined body that exhibits high and stable joining strength, and a joining method therefor.SOLUTION: A method for joining fiber reinforced thermoplastics in the present invention includes joining FRTPs through a thermoplastics sheet, wherein the FRTP, and FRTP used in the thermoplastics sheet are the same thermoplastics, and an interlayer mainly composed of the thermoplastics sheet has a thickness of 5-500μm.</p> |