A metal-air battery is disclosed. The battery includes a sodium anode and an air cathode. The battery further includes a solid electrolyte. The sodium anode may be a molten sodium anode, and the solid electrolyte may be a beta alumina solid electrolyte. The battery has an operating temperature between 100° C and 200° C.
申请公布号
WO2014042761(A2)
申请公布日期
2014.03.20
申请号
WO2013US50615
申请日期
2013.07.16
申请人
BATTELLE MEMORIAL INSTITUTE
发明人
LU, XIAOCHUAN;LEMMON, JOHN P.;LI, GUOSHENG;SPRENKLE, VINCENT L.