摘要 |
A process for producing an ejection orifice forming member including the steps of forming a laminate including a first negative photosensitive resin layer that contains a first photoacid generator, and a second negative photosensitive resin layer that is formed on the first negative photosensitive resin layer and contains a second photoacid generator; forming a first latent image and a second latent image on the first negative photosensitive resin layer and the second negative photosensitive resin layer, respectively, by collectively subjecting the first negative photosensitive resin layer and the second negative photosensitive resin layer to exposure; performing a heat treatment after the exposure; and forming the ejection orifice by a development treatment. The first photoacid generator in the first latent image has an acid diffusion length greater than the acid diffusion length of the second photoacid generator in the second latent image. |