摘要 |
PROBLEM TO BE SOLVED: To provide a polyester film for a molded member that improves moldability, productivity, and molding cycle by improving a temperature rising rate of the polyester film, and that further has beauty of appearance after molding.SOLUTION: A polyester film for a molded member is a polyester film in which a minimum value of transmittance in a wavelength of 700-2,500 nm is at most 80% and a melting point is 240-260°C, and is such that a rupture stress of the film after being heated for 180 seconds by an infrared heater is at least 40 and less than 100 MPa for both a longitudinal direction and a width direction. |