摘要 |
<p>PURPOSE: A finishing material composition of plastering interior of a building is provided to improve the effects of deodorization, antibiotic, and deodorization characteristic in indoor for a long term by using kaolin, titanium dioxide, calcined shell powder, and phytoncide. CONSTITUTION: A finishing material composition of plastering interior of a building comprises the following steps: Kaolin is classified into multiple granularity sizes through sieve disaseembly process; and 65+/-10 parts by weight of a large granule kaolin and a small granule kaolin, 17+/-3 parts by weight of E.V.A resin, 5+/-1 parts by weight of titanium dioxide, 3+/-1 parts by weight of calcined shell powder, and water are mixed. The granule size of the Kaolin classification step may be 20+/-5 meshes, 30+/-5 meshes, 40+/-5 meshes, 50+/-5 meshes, 60+/-5 meshes, 70+/-5 meshes, 80+/-5 meshse, 90+/-5 meshse, and 100+/-5 meshse. The water is provided to the filtrate of loess suspension. Based on 100kg of plastering composition, 10-30g of phytoncide is added.</p> |