摘要 |
The invention solves the problem of the manner of obtainment of mass for production of shaped construction elements. The manner consists of the fact, that in the mechanical mixer a ceramic granulate is placed, preferably in the form of pearlite and is soaked, preferably with water until complete soaking of the granulate and is mixed with the binding agent until obtainment of the situation, where each loose grain (1) of the granulate is coated with a layer of moist binding agent, creating a coating (2) around the grain. Priorly prepared moulds are filled with the obtained mass. The mass for production of shaped construction elements consists of 15-25% of bond weight, preferably in the form of pearlite, 35-45% of binding agent weight, preferably in the form of plaster with improved resistance parameters and 35-45% of water weight.
|