摘要 |
The invention relates to a molded plastic body (1) which is produced from a cured reaction mixture (2). Said reaction mixture (2) is pourable in the non-cured state and comprises 50 to 90 % by weight, based on the reaction mixture (2), of an inorganic particulate filler (3), a cross-linking agent (4), and 10 to 50 % by weight, based on the reaction mixture (2), of a binder solution (5). Said binder solution (5) comprises a monomer and a polymer dissolved therein. The inventive molded plastic body is characterized in that the percentage of the cross-linking agent (4) admixed to the binder solution (5) is more than 10 % by weight based on the percentage of the monomer in the binder solution (5). The invention also relates to a method for producing the molded plastic body. |