发明名称 HIGH SILICON BEARING DUAL PHASE STEELS WITH IMPROVED DUCTILITY
摘要 <p>A dual phase steel (martensite + ferrite) having a tensile strength of at least 980 MPa, and a total elongation of at least 15%. The dual phase steel may have a total elongation of at least 18%. The dual phase steel may also have a tensile strength of at least 1180 MPa. The dual phase steel may include between 0.5-3.5 wt.% Si, and more preferably between 1.5-2.5 wt.% Si.</p>
申请公布号 WO2013082171(A1) 申请公布日期 2013.06.06
申请号 WO2012US66877 申请日期 2012.11.28
申请人 JUN, HYUN JO;POTTORE, NARAYAN S.;FONSTEIN, NINA MICHAILOVNA;ARCELORMITTALLNVESTIGACION Y DESARROLLO S.L. 发明人 JUN, HYUN JO;POTTORE, NARAYAN S.;FONSTEIN, NINA MICHAILOVNA
分类号 C22C38/00;C22C38/02;C22C38/04;C22C38/06 主分类号 C22C38/00