MANUFACTURING METHOD OF LITHIUM NICKEL COBALT ALUMINIUM COMPOSITE OXIDE, LITHIUM NICKEL COBALT ALUMINIUM COMPOSITE OXIDE MADE BY THE SAME, LITHIUM SECONDARY BATTERY COMPRISING THE SAME |
摘要 |
PURPOSE: A manufacturing method of a composite oxide of a lithium-nickel-cobalt-aluminum composite is provided to stably obtain the lithium-nickel-cobalt-aluminum composite with a particle diameter of 10-20 micron and tab density of 2.5-2.6 g/cc, using a spray drying method. CONSTITUTION: A manufacturing method of a composite oxide of a lithium-nickel-cobalt-aluminum composite comprises a step of mixing a nickel compound, cobalt compound, and aluminum compound in a solvent, by stoichiometry, and dispersing the mixture; a step of manufacturing slurry by wet drying the dispersed mixture to reach the average particle size of 0.3 micron or less; a step of spraying and drying the slurry; a step of mixing a lithium compound with the dry slurry; and a step of sintering the mixture. [Reference numerals] (AA) Example 1; (BB) Comparative example 1; (CC) Comparative example 2 |
申请公布号 |
KR20130059158(A) |
申请公布日期 |
2013.06.05 |
申请号 |
KR20110125324 |
申请日期 |
2011.11.28 |
申请人 |
POSCO ES MATERIALS CO., LTD. |
发明人 |
KIM, YOO JUNG;LEE, MIN YOUNG;KO, HYOUNG SHIN |
分类号 |
H01M4/1391;H01M4/525;H01M10/052 |
主分类号 |
H01M4/1391 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|