发明名称 Verfahren zum Herstellen einer hoch-korrosionsbestaendigen und warmfesten Nickel-Chrom-Molybdaen-Legierung mit erhoehter Bestaendigkeit gegen interkristalline Korrosion
摘要 A nickel-chromium-molybdenum alloy which retains its corrosion-resistance after welding contains in percentage by weight <TABS:0956166/C3/1> The alloy is prepared from silicon-free materials and is de-oxidized with a silicon-free metal selected from Ca, Mg, Ba, Sr. Silicon-free master alloys of these metals, preferably with nickel, or silicon-free titanium master alloy, may also be used. Post-weld annealing at 1120 DEG C., followed by air cooling, is referred to.
申请公布号 DE1210566(B) 申请公布日期 1966.02.10
申请号 DE1961B061993 申请日期 1961.04.01
申请人 BADISCHE ANILIN- & SODAFABRIK AKTIENGESELLSCHAFT 发明人 SCHEIL DR. ERICH;CLASS DIPL.-ING. DR. IMMANUEL;GRAEFEN DR. HUBERT
分类号 C22B23/06;B23K35/30;C22C19/05 主分类号 C22B23/06