PURPOSE: A method for preparing environmentally-friendly natural mineral composite functional solution is provided to remove odor by modifying large water molecule structure to small molecular structure and to improve water quality. CONSTITUTION: A method for preparing environmentally-friendly natural mineral composite functional solution comprises: a step of mixing 7.5-12.5 weight% of germanium powder, 6.5-12.3 weight% of elvan powder, 10.5-12.2 weight% of zeolite powder in 63-75.5 weight% of water and stirring; a step of precipitating the mixture for more than 24 hours to obtain supernatant containing mineral; a step of filtering supernatant to remove foreign materials; a step of eluting water soluble calcium carbonate for 20-30 minutes to contain water soluble calcium carbonate; and a step of circulating permanent magnets for 30-60 minutes. |