摘要 |
FIELD: chemistry.SUBSTANCE: composition contains the following (pts.wt): epoxide oligomer 29-35, oligoamidoamide 4-7, hollow glass microspheres 25-33, ammonium phosphate 15-21.5, aliphatic amine 8-12, catalyst 0.5-1, rubber 3-6 and powdered filler 2.5-3.5.EFFECT: invention enables to obtain a polymer composition which solidifies in 6-12 hours at room temperature and has high compression strength and impact viscosity.7 cl, 3 tbl, 3 ex |