A method for applying a low residual stress damping coating to a surface of a substrate is provided. The method includes heating a ferromagnetic damping material in powder form such that the ferromagnetic damping material is at least partially molten. Next, the at least partially molten ferromagnetic damping material is directed at a surface of the substrate at an application velocity so that it adheres to the surface of the substrate to create a ferromagnetic damping coating on the surface of the substrate, resulting in a coated substrate. The ferromagnetic damping coating has a balanced coating residual stress, including a tensile quenching stress component and a compressive peening stress component. The balanced coating residual stress is within a range of ± 50 MPa without having to subject the coated substrate to a high temperature annealing process. The resulting coated substrate exhibits a high damping capacity. |