摘要 |
FIELD: metallurgy. ^ SUBSTANCE: method to manufacture cold-deformed pipes from double-phase alloys based on titanium includes ingot smelting, ingot forging in a -area or - and +-area with forging completion in the +-area into an intermediate blank with the specified forging reduction. The intermediate blank is produced with forging reduction of at least 1.35, a block is made from the intermediate blank, which is pressed into a billet and thermally treated at the temperature that is by 30-40C below the temperature of Tint, and them the billet is rolled with intermediate surface treatment, etching and thermal treatment. Drawing in process of rolling is defined using the following formula. ^ EFFECT: produced pipes are characterised by high physical-mechanical properties due to exclusion of formation of grain-to-grain microcracks. ^ 4 tbl, 1 ex |