发明名称 |
CERAMIC BLOCK FOR TOOTH RESTORATION AND MANUFACTURING METHOD OF THE SAME |
摘要 |
PURPOSE: A method for manufacturing a ceramic dental restoration material is provided to suppress sensitive teeth and to teeth abrasion. CONSTITUTION: A dental restoration material contains 50-80 wt% of P_2O_5, 8-30 wt% of CaCO_3, 3-18 wt% of Al_2O_3, 0.01-5 wt5 of Li_2CO_3, 0.01-7 wt% of TiO_2, 0.01-5 wt% of ZrO, 0.001-2 wt% of SiO_2, 0.001-2 wt% of NiO, and 0.0001-1.5 wt% of Fe_2O_3. A method for manufacturing the dental restoration material comprises: a step of weighing the ingredients; a step of mixing the ingredients and pulverizing the ingredients; a step of performing the pulverized ingredients by thermal treatment; and a step of quickly cooling the resultant. [Reference numerals] (AA) Temperature; (BB) Time
|
申请公布号 |
KR20120108382(A) |
申请公布日期 |
2012.10.05 |
申请号 |
KR20110026160 |
申请日期 |
2011.03.24 |
申请人 |
M&C DENTAL CO., LTD.;KOREA INSTITUTE OF CERAMIC ENGINEERING AND TECHNOLOGY |
发明人 |
KIM, KYOUNG HUN;PARK, JOO SEOK;CHAE, JAE HONG;KIM, TAE KWAN;AHN, JONG PIL;JEONG, SUNG MIN;PARK, YOON WOO;LEE, CHANG TAEK |
分类号 |
A61K6/033;A61K6/02;A61K6/04 |
主分类号 |
A61K6/033 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|