发明名称 GLASS COATING AGENT
摘要 <P>PROBLEM TO BE SOLVED: To provide a normal temperature glass coating agent which can be applied to the surface of a metal such as stainless steel at a so-called normal temperature of 200&deg;C or less to thereby easily obtain the metal excellent in weather resistance, antifouling property, and flame retardancy. <P>SOLUTION: The normal temperature glass coating agent contains boron ions and halogen ions as a catalyst required for making oxides and is composed of a single composition or a composite composition of a hydrolyzable organometallic compound dissolved in an alcohol. When the glass coating agent is applied to the surface of a metal plate, it can be dried at a so-called normal temperature of 200&deg;C or less, and the metal surface can be made excellent in weather resistance, antifouling property, and flame retardancy. <P>COPYRIGHT: (C)2012,JPO&INPIT
申请公布号 JP2012180544(A) 申请公布日期 2012.09.20
申请号 JP20110043133 申请日期 2011.02.28
申请人 BOKUTO KASEI KOGYO KK;MORISANE TOSHITOMO 发明人 OIDA MASARU;OSHIMA KOJI;MORISANE TOSHITOMO
分类号 C23D5/02;B05D7/14;B32B15/01;C03C8/14;C09D1/00;C09D183/04 主分类号 C23D5/02
代理机构 代理人
主权项
地址