发明名称 NICKEL-COBALT-MANGANESE COMPLEX HYDROXIDE PARTICLES AND METHOD FOR PRODUCING SAME, POSITIVE ELECTRODE ACTIVE MATERIAL FOR NONAQUEOUS ELECTROLYTE SECONDARY BATTERY AND METHOD FOR PRODUCING SAME, AND NONAQUEOUS ELECTROLYTE SECONDARY BATTERY
摘要 An object of the present invention is to provide nickel cobalt manganese composite hydroxide particles having a small particle diameter and a uniform particle size distribution, and a method for producing the same. [Solution] A method for producing a nickel cobalt manganese composite hydroxide by a crystallization reaction is provided. The method includes: a nucleation step of performing nucleation by controlling a pH of an aqueous solution for nucleation including metal compounds containing nickel, cobalt and manganese, and an ammonium ion donor to 12.0 to 14.0 in terms of the pH as measured at a liquid temperature of 25° C. as a standard; and a particle growth step of growing nuclei by controlling a pH of an aqueous solution for particle growth containing nuclei formed in the nucleation step to 10.5 to 12.0 in terms of the pH as measured at a liquid temperature of 25° C. as a standard.
申请公布号 KR20120099098(A) 申请公布日期 2012.09.06
申请号 KR20127016853 申请日期 2010.12.02
申请人 TOYOTA JIDOSHA KABUSHIKI KAISHA;SUMITOMO METAL MINING CO., LTD. 发明人 TOYA HIROYUKI;IMAIZUMI SHIN;MORI KENSAKU;FUKUI ATSUSHI;IKEUCHI KENJI;RYOSHI KAZUOMI;OSAKO TOSHIYUKI;NAGAI HIROKI
分类号 H01M4/525;C01G53/00;H01M4/505;H01M10/05 主分类号 H01M4/525
代理机构 代理人
主权项
地址