发明名称 |
METHOD FOR MANUFACTURING STEEL SHEET |
摘要 |
PURPOSE: A steel plate manufacturing method is provided to improve the deep-drawability of a steel plate by reducing the amount of solute carbon and solute nitrogen. CONSTITUTION: A steel plate manufacturing method comprises the steps of: hot-rolling a slab at a temperature lower than the Ar3 temperature, cooling the hot-rolled product first at a cooling rate of 20°C/sec-50°C/sec, maintaining the cooled hot-rolled product in a temperature range of 720°C-650°C, cooling the hot-rolled product secondly at a cooling rate of 20°C/sec-50°C/sec, and rolling the cooled hot-rolled product into a coil in a temperature range of 500°C-300°C temperature range.
|
申请公布号 |
KR20120032836(A) |
申请公布日期 |
2012.04.06 |
申请号 |
KR20100094377 |
申请日期 |
2010.09.29 |
申请人 |
HYUNDAI STEEL COMPANY |
发明人 |
KIM, DONG YONG;PARK, JI HWAN;YOON, CHI SANG |
分类号 |
C21D8/02;B21B1/26;C21D9/46;C22C38/00 |
主分类号 |
C21D8/02 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|