<p>The present invention relates to a method for producing a cured product of a thermosetting resin composition, the method including: heating a thermosetting resin composition including the following ingredients (A) to (C) at a temperature of 100 to 200°C for 1 to 60 minutes; and then further heating the thermosetting resin composition at a temperature of 220 to 350°C for 10 to 6,000 minutes, thereby curing the thermosetting resin composition: (A) an allylated phenol resin; (B) an epoxy resin; and (C) a curing accelerator.</p> |