PROBLEM TO BE SOLVED: To provide a resin molded product having a calm texture such as a "Nanbu iron".SOLUTION: In the resin molded product including a matrix made of resin, a coloring material dispersed in the matrix and a particle-shaped brightness material dispersed in the matrix, the coloring material has ≥20 mμ average particle diameter, ≥5 pts.wt. coloring material is included to 100 pts.wt. resin and the coloring material and the particle-shaped brightness material are dispersed so that total light transmittance in wavelength of wavelength λ=400 to 800 nm in a position of 1.5 mm depth from the surface of the resin molded product is <0.01%. |