发明名称 Method of production of grain-oriented electrical steel sheet having a high magnetic flux density
摘要 In a production of grain-oriented electrical steel sheet that is heated at a temperature of not higher than 1350° C., (a) the hot-rolled sheet is heated to a prescribed temperature of 1000° C. to 1150° C., and after recrystallization is annealed for a required time at a lower temperature of 850° C. to 1100° C., or (b) in the hot-rolled sheet annealing process decarburization is conducted to adjust the difference in the amount of carbon before and after decarburization to 0.002 to 0.02 mass %. In the temperature elevation process used in the decarburization annealing of the steel sheet, heating is conducted in the temperature range of 550° C. to 720° C. at a heating rate of at least 40° C./s, preferably 75 to 125° C./s, utilizing induction heating for the rapid heating used in the temperature elevation process in decarburization annealing.
申请公布号 US7976645(B2) 申请公布日期 2011.07.12
申请号 US20070227459 申请日期 2007.05.23
申请人 NIPPON STEEL CORPORATION 发明人 USHIGAMI YOSHIYUKI;FUJII NORIKAZU;KUMANO TOMOJI
分类号 H01F1/147 主分类号 H01F1/147
代理机构 代理人
主权项
地址