发明名称 |
METHOD OF PREPARING WEAR-RESISTANT COMPOSITION |
摘要 |
FIELD: chemistry. ^ SUBSTANCE: method is realised by cold pressing under specific pressure of 12.5 MPa with subsequent saturation in engine oil M-8B at temperature 150C for 24 hours and sintering at temperature 3705C. The invention enables to produce large group of cheap readily available materials with good structural and anti-frictional properties, capable of prolonged operation in self-lubrication mode in friction assemblies as friction bearings and movable sealants, including in cryogenic engineering. ^ EFFECT: method significantly increases wear-resistance and load capacity of articles made using the disclosed technique. ^ 2 cl, 4 tbl, 16 ex |
申请公布号 |
RU2421480(C2) |
申请公布日期 |
2011.06.20 |
申请号 |
RU20090132447 |
申请日期 |
2009.08.27 |
申请人 |
UCHREZHDENIE ROSSIJSKOJ AKADEMII NAUK INSTITUT PROBLEM NEFTI I GAZA SIBIRSKOGO OTDELENIJA RAN;FEDERAL'NOE GOSUDARSTVENNOE AVTONOMNOE OBRAZOVATEL'NOE UCHREZHDENIE VYSSHEGO PROFESSIONAL'NOGO OBRAZOVANIJA "SEVERO-VOSTOCHNYJ FEDERAL'NYJ UNIVERSITET IM. M.K. AMMOSOVA" |
发明人 |
OKHLOPKOVA AJTALINA ALEKSEEVNA;PETROVA PAVLINA NIKOLAEVNA;FEDOROV ANDREJ LEONIDOVICH;MOROVA LILIJA JAG'JAEVNA;NIKIFOROV LEONID ALEKSANDROVICH |
分类号 |
B29B11/12;B29B11/16;B29C71/00;C08J5/16;C08L27/18 |