摘要 PROBLEM TO BE SOLVED: To certainly suppress the occurrence of a crack, breakage or the like in the case of the insert molding of a component. SOLUTION: When the component 2 is subjected to insert molding in a resin, the resin is injected so as not to cause welding at the thinnest part of the resin (resin part D) in the periphery of the component 2. Moreover, in a case that the resin contains a fibrous filter (f), the resin is injected so that the fibrous filler f is oriented in the direction almost crossing the minimum cross section s of the resin part D. Further, in a case that the component 2 is a rare earth metal magnet and has the coefficient of negative thermal expansion, the resin is injected from the direction almost parallel to a direction becoming largest in the productαL of the dimension L of the component 2 and the coefficientαof thermal expansion in the dimensional direction of the component 2. COPYRIGHT: (C)2006,JPO&NCIPI
申请公布号 JP4692007(B2) 申请公布日期 2011.06.01
申请号 JP20050038977 申请日期 2005.02.16
申请人 发明人
分类号 B29C45/14;B29C33/12;B29K101/10;B29K105/12 主分类号 B29C45/14
代理机构 代理人
主权项
地址