发明名称 Low temperature co-fired ceramic material, low temperature co-fired ceramic body, and multilayer ceramic substrate
摘要 <p>A low temperature co-fired ceramic material includes a SiO 2 -BaO-Al 2 O 3 -based primary component, and, as secondary components, 0.044 to 0.077 parts by weight of iron in terms of Fe 2 O 3 and 0.30 to 0.55 parts by weight of zirconium in terms of ZrO 2 relative to 100 parts by weight of the siO 2 -BaO-Al 2 O 3 -based primary component. The SiO2-BaO-Al 2 O 3 -based primary component preferably includes 47% to 60% by weight of SiO 2 , 20% to 42% by weight of BaO, and 5% to 30% by weight of Al 2 O 3 .</p>
申请公布号 EP2325150(A1) 申请公布日期 2011.05.25
申请号 EP20100187362 申请日期 2010.10.13
申请人 MURATA MANUFACTURING CO., LTD. 发明人 YOKOYAMA, TOMOYA;KAWADA, YUZO;BABA, AKIRA;KAWAKAMI, HIROMICHI;KATO, ISAO
分类号 C04B35/195;B32B18/00;H01L23/15 主分类号 C04B35/195