发明名称 |
WATER-BASED SLURRY COMPOSITION FOR MAKING ENVIRONMENTAL BARRIER COATING AND ENVIRONMENTAL BARRIER COATING COMPRISING THE SAME |
摘要 |
<P>PROBLEM TO BE SOLVED: To provide an environmental barrier coating to protect CMC (Ceramic Matrix Composite) from the high temperature steam environments present in gas turbine engines. <P>SOLUTION: The environmental barrier coating includes: at least one transition layer 16 made from a transition layer slurry comprising: from about 1 wt.% to about 99.9 wt.% water; from about 0.1 wt.% to about 72 wt.% primary transition material; from about 0.1 wt.% to about 59.3 wt.% Lnb rare earth metal slurry sintering aid; at least one transition layer 16 produced from a transition layer slurry composed of about 0.1 wt.% to about 20.6 wt.% SiO<SB>2</SB>slurry sintering aid; optionally, any one or more of: an outer layer 20 made from an outer layer slurry comprising: from about 1 wt.% to about 99.9 wt.% water; and from about 0.1 wt.% to about 72 wt.% primary outer material; and a compliant layer 18 made from a pliable layer slurry comprising: from about 1 wt.% to about 99.9 wt.% water; and from about 0.1 wt.% to about 72 wt.% primary pliable material. <P>COPYRIGHT: (C)2011,JPO&INPIT |
申请公布号 |
JP2011051882(A) |
申请公布日期 |
2011.03.17 |
申请号 |
JP20100169896 |
申请日期 |
2010.07.29 |
申请人 |
GENERAL ELECTRIC CO |
发明人 |
KIRBY GLEN HAROLD;BOUTWELL BRETT ALLEN;SUBIT JESSICA L |
分类号 |
C04B35/622;C04B41/87;C04B41/89;F01D5/28;F01D25/00;F02C7/00;F02C7/30 |
主分类号 |
C04B35/622 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|