发明名称 IMPREGNATED BIT WITH INCREASED BINDER PERCENTAGE
摘要 Control of the carbide volume in the matrix in an impregnated bit is accomplished by coating the hard particles in the matrix to space them further apart to increase the soft binder percentage in a controllable manner. The softer binder due to lower volume content of hard particles allows more rapid matrix wear in the softer formations to allow more diamond grit to cut better before getting flat spots and to be replaced faster with additional diamond grit further into the matrix as the higher content of the softer binder and the softer coating on the hard particles in the matrix promotes more effective cutting with more frequent emergence of diamond grit on the bit face as cutting progresses.
申请公布号 WO2010123906(A3) 申请公布日期 2011.03.03
申请号 WO2010US31759 申请日期 2010.04.20
申请人 BAKER HUGHES INCORPORATED;SCOTT, DAN, E. 发明人 SCOTT, DAN, E.
分类号 E21B10/46;B22F7/06;C22C29/08 主分类号 E21B10/46