发明名称 Verfahren zum Herstellen eines Bauteils aus einem lufthärtbaren Stahl und ein damit hergestelltes Bauteil
摘要 <p>A component of an air-hardenable steel composed of (contents in mass %): C<0.20; Al<0.08; Si<1.00; Mn 1.20 to <2.50; P<0.020; S<0.015; N<0.0150; Cr 0.30 to <1.5; Mo 0.10 to <0.80; Ti 0.010 to <0.050; V 0.03 to <0.20; B 0.0015 to <0.0060, with the remainder being iron including the usual elements present in steel, is produced by heating a hot- or cold-rolled steel sheet or steel tube section to a temperature ofθblank=800 to 1050° C. and then forming the sheet or tube into a component in a forming tool. After removal from the tool, the component is cooled down in air while the component still has a temperature aboveθremoval=200° C. and below 800° C. The component achieves the required mechanical properties during air-cooling.</p>
申请公布号 DE102010024664(A1) 申请公布日期 2011.02.17
申请号 DE20101024664 申请日期 2010.06.18
申请人 SALZGITTER FLACHSTAHL GMBH 发明人 BRAUN, MICHAEL;EGGERS, UWE;SCHAEFFNER, CORD;SCHOETTLER, JOACHIM;LUTHER, FRIEDRICH;MUETZE, STEFAN;OTTO, MANUEL;REIER, THORSTEN
分类号 C22C38/00;C21D7/00;C22C38/04 主分类号 C22C38/00
代理机构 代理人
主权项
地址
您可能感兴趣的专利