摘要 |
This flat mineral glass comprises a first free surface and a second free surface, and comprises groups of zones having a high refractive index (n2) and zones having a low refractive index (n1) which are formed in the thickness of the flat glass between the first and second free surfaces, over a depth of between 1 and 1000 μm starting from the first free surface. These high-index zones and low-index zones alternate along a direction transverse to the thickness direction of the glass between the first and second free surfaces, the high-index zones flaring out from the first free surface toward the second free surface, and the envelope surfaces of the high-index zones making an angle (&thetas;) of at least 65° with respect to the first free surface. |