发明名称 BIO-CO-CR-MO ALLOY WITH ION ELUTION SUPPRESSED BY STRUCTURE CONTROL, AND PROCESS FOR PRODUCING SAME
摘要 This invention provides a technique for rendering bio-toxicity such as allergy toxicity derived from Ni trace impurity, i.e., nickel toxicity, which is unavoidably present in a bio-Co—Cr—Mo alloy or an Ni-free stainless steel alloy unharmful, characterized in that an element selected from the group consisting of the group 4, 5 and 13 elements of the periodic table, particularly an element selected from the group consisting of the group 4 elements of the periodic table, is added to the alloy composition. The additive element is preferably an element selected from the group consisting of zirconium and titanium, more preferably zirconium.
申请公布号 US2011023661(A1) 申请公布日期 2011.02.03
申请号 US20100891622 申请日期 2010.09.27
申请人 CHIBA AKIHIKO;KUROSU SHINGO;NOMURA NAOYUKI 发明人 CHIBA AKIHIKO;KUROSU SHINGO;NOMURA NAOYUKI
分类号 C21B15/00;C22C1/02 主分类号 C21B15/00