发明名称 連続繊維補強材及び連続繊維補強材の製造方法
摘要 PROBLEM TO BE SOLVED: To provide a continuous fiber reinforcement excellent in adhesion performance and tensile strength.SOLUTION: In a continuous fiber reinforcement, diameters at spots having larger sectional areas than the average sectional area of a test piece with respect to a test piece having an optional length 1 meter were measured, and when the average value of top large-diameter 5 points is represented by x, the ratio x/y to the average diameter y of the test piece is ≥1.05 to ≤2.00.
申请公布号 JP5966390(B2) 申请公布日期 2016.08.10
申请号 JP20120017973 申请日期 2012.01.31
申请人 東洋紡株式会社 发明人 大林正佳;野村幸弘
分类号 C04B16/06;C04B14/38;E04C5/07 主分类号 C04B16/06
代理机构 代理人
主权项
地址