摘要 Metals for use in glass-making furnaces and which are susceptible to oxidation at furnace operating temperatures, especially iridium or molybdenum, are protected by applying at least (200) microns thickness of a coating formed of metal oxide particles in a metal oxide matrix. Oxidation, measured by weight loss, is significantly reduced.