发明名称 COOLING METHOD AND COOLING DEVICE FOR HOT-ROLLED STEEL SHEETS
摘要 <p>Provided is a method for cooling hot-rolled steel sheets after a final rolling. Using cooling water at a flow rate between 4 m³/m²/min and 10 m³/m²/min, the hot-rolled steel is cooled from a first temperature between 600°C and 650°C to a second temperature less than or equal to 450°C. At least 80% of the surface area of the surface being cooled is directly impacted by a jet of the aforementioned cooling water.</p>
申请公布号 WO2010131467(A1) 申请公布日期 2010.11.18
申请号 WO2010JP03238 申请日期 2010.05.13
申请人 NIPPON STEEL CORPORATION;SERIZAWA, YOSHIHIRO;NISHIYAMA, YASUHIRO;OGAWA, SHIGERU;IDA, SHINJI;NIKAIDOH, HITOSHI;YOSHII, ISAO;HISHINUMA, NORIYUKI;KISHIMOTO, TETSUO;TAKAGI, NOBUHIRO 发明人 SERIZAWA, YOSHIHIRO;NISHIYAMA, YASUHIRO;OGAWA, SHIGERU;IDA, SHINJI;NIKAIDOH, HITOSHI;YOSHII, ISAO;HISHINUMA, NORIYUKI;KISHIMOTO, TETSUO;TAKAGI, NOBUHIRO