PURPOSE: A nanofiber dyeing method is provided to maintain all the characteristic of the nanofiber, thereby reducing the decoloration of the dyed object. CONSTITUTION: Nano fiber is dipped in the dyeing mixture liquid of 30 degree. The dyeing mixture solution maintain in 70 degree. The nanofiber is dyed for the half an hour. The nanofiber is cleaned with the warm water. The nanofiber is dipped in the adherence liquid. The temperature of the adherence liquid is increased one degree per minute. If the temperature is 70 degrees, the reaction of the nanofiber maintains for 20 minutes. If the nanofiber is arranged in the wrap tenter, the thermal process of nanofiber operates.