发明名称 Method of making copper wire rod with low semi-softening temperature, method of making copper wire and copper wire
摘要 A method of making a copper wire rod with low semi-softening temperature includes melting a raw material copper to have a copper melt, adjusting concentrations of oxygen and sulfur included in the copper melt to be not more than 20 ppm and not more than 6 ppm, respectively, continuously casting the adjusted copper melt at temperature not higher than 1120° C. to have a cast bar, and hot-rolling the cast bar in a temperature range of 850° C. to 550° C.
申请公布号 US2010230069(A1) 申请公布日期 2010.09.16
申请号 US20100659453 申请日期 2010.03.09
申请人 HITACHI CABLE, LTD. 发明人 AOYAMA SEIGI;SUMI TORU
分类号 B22D11/00 主分类号 B22D11/00