发明名称 |
Method of producing a cold temperature high toughness structural steel tubing |
摘要 |
An apparatus (10) includes a low-carbon steel tube (24). The low-carbon steel tube (24) yields plastically more than about 5% before fracturing at temperatures down to about−40° C. when stress is applied to the low-carbon steel tube sufficient to cause the low carbon steel tube to so yield.
|
申请公布号 |
US7776160(B2) |
申请公布日期 |
2010.08.17 |
申请号 |
US20030726961 |
申请日期 |
2003.12.03 |
申请人 |
TRW AUTOMOTIVE U.S. LLC;SUMITOMO METAL INDUSTRIES LTD. |
发明人 |
ERIKE ERIC C. |
分类号 |
C21D7/13;B60R21/26;B60R21/264;C21D1/42;C21D8/10;C21D9/08;C22C38/04;C22C38/18;F17C1/00;F17C1/16 |
主分类号 |
C21D7/13 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|