Hardened spring steel, spring element and method for manufacturing a spring element |
摘要 |
The tempered spring steel (1) comprises an edge layer (2), within which the hardness of the interior outwardly drops and which is softened by a heat treatment and/or induction heating, where the spring steel is tempered in its entire cross-section. The edge layer has a thickness of 500-800 mu m, a hardness of 590 HV up to in a depth of 300-800 mu m, and a hardness of 500 HV from a depth of 50 mu m. The spring steel has a core region (3), which begins in a depth of 800 mu m and has a hardness of 600 HV. An independent claim is included for a method for producing a spring steel. |
申请公布号 |
EP2192201(A1) |
申请公布日期 |
2010.06.02 |
申请号 |
EP20090014562 |
申请日期 |
2009.11.23 |
申请人 |
MUHR UND BENDER KG |
发明人 |
NEUBRAND, JOERG, DR.-ING.;HARTWIG, MAIK |
分类号 |
C21D1/02;C21D8/06;C21D9/02 |
主分类号 |
C21D1/02 |