摘要 <P>PROBLEM TO BE SOLVED: To provide a method for melting solid-iron source in a molten iron carrier by which even in the case of beforehand laying dephosphorized bare metal and/or desulfurized bare metal recovered at the slag-off time after dephosphorization and/or desulfurization of the molten iron, there is no possibility of phreatic explosion. <P>SOLUTION: A technique with which the solid iron source is beforehand laid into the molten iron carrying vessel, the molten iron from a blast furnace is received and this solid iron source is melted by using the sensible heat and stirring force, is improved. In this method, as the solid-iron source, the dephosphorized bare metal and/or the desulfurized bare metal which are agglomerated and solidified at the size of 200-1,500mm and recovered in the high temperature state of 100-600&deg;C are used in the slag generated with the dephosphorization and/or the desulfurization of the molten during leaving the slag in the yard. In this time, it is preferable to beforehand lay the dephosphorized bare metal and/or the desulfurized bare metal into the molten iron carrier by using a heat-resistant hydraulic-type heavy machine. <P>COPYRIGHT: (C)2006,JPO&NCIPI
申请公布号 JP4442369(B2) 申请公布日期 2010.03.31
申请号 JP20040253183 申请日期 2004.08.31
申请人 发明人
分类号 C21C1/02 主分类号 C21C1/02
代理机构 代理人
主权项
地址
您可能感兴趣的专利