<p>A method comprising contacting a support with a chromium-containing compound and a tin-containing compound to produce a catalyst precursor, and activating the catalyst precursor in a temperature range of from about 400 ?C to about 700 ?C to produce a polymerization catalyst. A method comprising contacting a support with a chromium-containing compound and a tin-containing compound to produce a catalyst precursor, activating the catalyst precursor in a temperature range of from about 400 ?C to about 700 ?C to produce a polymerization catalyst, and contacting the polymerization catalyst with ethylene in a reaction zone under suitable reaction conditions to form polyethylene wherein the molecular weight distribution of the polyethylene is broadened. ??</p>
申请公布号
WO2009134361(A1)
申请公布日期
2009.11.05
申请号
WO2009US02594
申请日期
2009.04.29
申请人
CHEVRON PHILLIPS CHEMICAL COMPANY LP;MCDANIEL, MAX, P.;COLLINS, KATHY, S.