Degreasing method for aluminium hard foil, aluminium hard foil, aluminium hard foil electrode member, and lithium ion secondary battery using said member |
摘要 |
An aluminum hard foil is degreased without reducing the hardness to improve the coating performance of coating material. A foil-rolled aluminum foil is subjected to a low-temperature heat treatment for holding the aluminum foil at 80 to 160° C. for 1 hour or more. The low-temperature heat treatment is preferably performed by subjecting the aluminum foil to batch processing with the aluminum foil coiled.
|