摘要 |
<p>The method involves providing two subcomponents (2, 3), where the subcomponent (2) is made of a super-alloy i.e. nickel-based super alloy, and the subcomponent (3) is made of high-temperature resistant steel e.g. chromium steel of 10 weight percentage. The two subcomponents are joint-welded, where a weld seam (5) is formed between the two subcomponents. The weld seam is heated to a temperature that corresponds to 70 to 130 percentage of an annealing temperature of the high-temperature resistant steel.</p> |