发明名称 PROCEDEU DE PRELUCRARE A PIEILOR OVINE CU BLANA
摘要 In order to improve the binding of chrome during the tanning of furry-sheep skins, the tanning liquor contains 600% water to which 0.6-0.8% sodium-alumino-silicate was added in three steps through 6-8 hours under constant stirring. This renders a pretreatment step superfluous.
申请公布号 RO96394(A2) 申请公布日期 1989.02.28
申请号 RO19860125672 申请日期 1986.12.02
申请人 INSTITUTUL DE CERCETARI PIELARIE SI INCALTAMINTE,RO 发明人 NICOLAE EUGENIA,RO;COARA GHEORGHE,RO;GAIDAU CORNELIA,RO;SZABO ILEANA,RO;MAN IOAN,RO
分类号 C14C3/06;(IPC1-7):C14C3/06 主分类号 C14C3/06