发明名称 |
PROCEDEU PENTRU TRATAREA FIBRELOR KERATINICE |
摘要 |
Keratin based fibres especially wool are treated as follows: The material is soaked and chlorinated. Residual chlorine is removed by reduction. This is followed by treatment with a reactive polyamide resin, softening, drying, preshrinking at 80-100 deg. C for 30 secs. This treatment reduces shrinking and ensures dimensional stability and improves feel. Chlorination takes place at pH 1-6 for 140 mins. at 5-30 deg. C. Resin treatment occurs at 40-50 deg. C at pH 7.2-7.8 for 20-40 min. 2.5% resin is applied based on fibre wt.
|
申请公布号 |
RO96310(A2) |
申请公布日期 |
1989.02.28 |
申请号 |
RO19860126226 |
申请日期 |
1986.12.27 |
申请人 |
INSTITUTUL DE CERCETARI TEXTILE,RO |
发明人 |
POPA MIRCEA D.,RO;MARCULESCU FLOAREA,RO;NAFORNITA COSTACHE,RO;MARCULESCU BOGDAN,RO |
分类号 |
D06M15/285;(IPC1-7):D06M15/285 |
主分类号 |
D06M15/285 |
代理机构 |
|
代理人 |
|
主权项 |
|