摘要 |
In one embodiment the present invention relates to a method for decreasing the gloss in a molded article comprising (i) at least one polycarbonate; (ii) at least one polyester; and (iii) at least one rubber modified thermoplastic resin; wherein the molded article exhibits a heat deflection temperature of at least 85° C. as measured at 1.8 MPa according to ISO 75, and a gloss value of less than or equal to about 3 as measured at an angle of 60°; and wherein the method comprises the step of preparing the article by molding using a textured mold at a mold temperature of greater than about 65° C. In other embodiments the present invention relates to molded articles.
|