摘要 <p><P>PROBLEM TO BE SOLVED: To provide an energy saving manufacturing method by which a reaction temperature and a reaction time are remarkably decreased using a manufacturing process such as normal pressure steam curing or rapid microwave-hydrothermal curing and to provide a hardened body exhibiting mechanical strength and dimensional stability. <P>SOLUTION: The energy saving method of manufacturing a coal ash hardened body includes: forming a mixed raw material containing the coal ash, a calcareous raw material, a reinforcing fiber, water and≤8 pts.wt. sodium hydroxide expressed in terms of a solid portion per 100 pts.wt. solid portion mixture of the siliceous raw material with the calcareous raw material; pre-drying at a prescribed temperature; solidifying by the normal pressure steam curing or the microwave-hydrothermal curing; and post-drying. The reaction temperature and the reaction/drying time are remarkably reduced by using microwave drying for the pre-drying and the post-drying. <P>COPYRIGHT: (C)2006,JPO&NCIPI</p>
申请公布号 JP2006117478(A) 申请公布日期 2006.05.11
申请号 JP20040307909 申请日期 2004.10.22
申请人 KAGAWA INDUSTRY SUPPORT FOUNDATION 发明人 CHIN SAIKA;KATO SHUNSAKU
分类号 C04B28/18;B28B1/00;B28B11/24;C04B14/38;C04B16/06;C04B18/10;C04B22/06;C04B40/02 主分类号 C04B28/18
代理机构 代理人
主权项
地址