发明名称 METHOD FOR PREVENTING HIGH STRENGTH CONCRETE FROM CRAZING DUE TO INITIAL DRYING
摘要 PROBLEM TO BE SOLVED: To effectively reduce crazing due to initial drying of high strength concrete without necessitating complicated ageing and without adding a large amount of admixtures such as a water reducing agent at the construction by using the high strength concrete. SOLUTION: The method comprises the steps of preparing high strength concrete of≥50 N/mm<SP>2</SP>compression strength by using coarse particle cement with a Blaine specific surface area of 1,000-2,400 cm<SP>2</SP>/g, and placing the high strength concrete to a site where the surface is exposed. Alternatively, the method comprises the steps of preparing first high strength concrete of≥50 N/mm<SP>2</SP>compression strength and placing it, and further preparing second high strength concrete of≥50 N/mm<SP>2</SP>compression strength by using coarse particle cement with a Blaine specific surface area of 1,000-2,400 cm<SP>2</SP>/g which is smaller than that of cement constituting the first high strength concrete, and placing the second high strength concrete on the surface of the first high strength concrete. COPYRIGHT: (C)2006,JPO&NCIPI
申请公布号 JP2006117439(A) 申请公布日期 2006.05.11
申请号 JP20040303733 申请日期 2004.10.19
申请人 SUMITOMO OSAKA CEMENT CO LTD 发明人 HARADA SHUSUKE;UCHIDA YOSHIO;NAKAMURA SHIRO;AOKI MAKI
分类号 C04B40/04;B28B1/16;C04B7/00;C04B28/02;E04G21/02 主分类号 C04B40/04
代理机构 代理人
主权项
地址