发明名称 METHOD FOR GRINDING LIGHT CALCIUM CARBONATE
摘要 PROBLEM TO BE SOLVED: To provide a method by which, in grinding in a high pH range, the viscosity of pigment slurry can be reduced with a smaller amount of a dispersant and causticized light calcium carbonate is efficiently wet-ground. SOLUTION: In the method for wet-grinding aggregated light calcium carbonate obtained in a causticizing step in a pulp making process by a sulfate method or soda method, the light calcium carbonate is slurried and the wet grinding is carried out in a slurry temperature range of 65-85°C so that the B type viscosity (60 rpm) of slurry of 73% concentration at a slurry temperature of 60°C is reduced to≤2,000 mPa s. COPYRIGHT: (C)2009,JPO&INPIT
申请公布号 JP2008247616(A) 申请公布日期 2008.10.16
申请号 JP20070087122 申请日期 2007.03.29
申请人 NIPPON PAPER INDUSTRIES CO LTD 发明人 MIYAWAKI SHOICHI;ARIMATSU HIROSHI;OCHI TAKASHI