发明名称 TiAl ALLOY SUPERIOR IN HIGH-TEMPERATURE CREEP CHARACTERISTICS AND MANUFACTURING METHOD THEREFOR
摘要 PROBLEM TO BE SOLVED: To provide a TiAl alloy which has superior high-temperature creep characteristics to a conventional one without impairing its toughness and lightweight properties. SOLUTION: The TiAl alloy has a composition comprising, by mass%, 31 to 34% Al, 0.1 to 0.7% Si, one or more elements of 0.1 to 15.0% Nb, 0.1 to 15.0% Mo, 0.1 to 15.0% W and 0.1 to 15.0% Ta so that the total amount can satisfy Nb+Mo+W+Ta≤15.0%, one or more elements of 0.1 to 3.0% Cr, 0.1 to 3.0% Mn and 0.1 to 3.0% V so that the total amount can satisfy Cr+Mn+V≤3.0%; 0.01 to 0.12% C and the balance Ti with unavoidable impurities, while satisfying the following expressions (1), (2) and (3): expression (1): value A (=0.15(Nb+Mo+W+Ta)+0.05(Cr+Mn+V)+0.95Si-5C)=0.8 to 3.0; expression (2): Al=(33.5-value A)±0.5; and expression (3): value B (=0.5Si+5C)=0.1 to 0.8. COPYRIGHT: (C)2008,JPO&INPIT
申请公布号 JP2008184665(A) 申请公布日期 2008.08.14
申请号 JP20070020164 申请日期 2007.01.30
申请人 DAIDO STEEL CO LTD 发明人 KOYANAGI SADAHIKO;NODA TOSHIHARU;SHIMIZU TETSUYA
分类号 C22C14/00;C22F1/00;C22F1/02;C22F1/18 主分类号 C22C14/00
代理机构 代理人
主权项
地址