摘要 A process is described for the recovery of nickel and cobalt from a nickeliferous laterite ore including the steps of: a) providing a nickeliferous laterite ore and separating that ore into its low magnesium limonite fraction and high magnesium saprolite fraction; b) treating the limonite fraction in acid solution in a primary high pressure leach step to produce a primary leach slurry; c) adding the saprolite fraction to the primary leach slurry to initiate precipitation of iron as goethite and/or hematite, while simultaneously releasing further acid from the iron precipitation, to effect a secondary atmospheric leach step, producing a secondary leach slurry; wherein all water used to prepare the ore slurries and/or acid solutions has an ionic composition that substantially avoids jarosite formation.
申请公布号 JP2008530356(A) 申请公布日期 2008.08.07
申请号 JP20070554392 申请日期 2006.02.13
申请人 发明人
分类号 C22B3/04;C22B3/44;C22B23/00 主分类号 C22B3/04