发明名称 METHOD TO DERIVE LOW MOLECULAR WEIGHT OLEFINS FROM LIGHT HYDROCARBON MATERIAL
摘要 FIELD: chemistry. ^ SUBSTANCE: invention relates to the method of low molecular weight olefins deriving, including pre-ward thermal pyrolysis of gasoline cut in warm pipes of tube heater with hydrocarbon product and amorphous coke derivation followed by thermal pyrolysis light hydrocarbon material in the same worm pipes of the tube heater. Furthermore, pre-ward thermal pyrolysis of gasoline cut is carried out at 760/835°C temperature and gasoline cut mass ratio is: water vapor =1.0:0.3/0.9 during 24/360 hours, besides pre-ward pyrolysis of gasoline cut is carried out in 2 stages: firstly, at 760/815°C temperature during 12/120 hours, than at 815/835°C temperature during 12/240 hours, and further pyrolysis of light hydrocarbon material is carried out at 780/855°C temperature and mass ratio of light hydrocarbon material is: water vapor =1.0:0.3/0.9, and broad fraction of light hydrocarbon material is used as light hydrocarbon material and it has the following composition, mass fraction, %: methane - 0,01/2,50, ethane - 0.50/4.50, propane - 5.0/95.00, total of C4 - 10.00/85.00; C5+ - 5.00/35.00. ^ EFFECT: time is increased for heater regeneration running during thermal pyrolysis of broad fraction of light hydrocarbon with high yield of low molecular weigh olefins. ^ 1 tbl, 6 ex
申请公布号 RU2326929(C1) 申请公布日期 2008.06.20
申请号 RU20070108599 申请日期 2007.03.07
申请人 OBSHCHESTVO S OGRANICHENNOJ OTVETSTVENNOST'JU "TOMSKNEFTEKHIM" (OOO "TOMSKNEFTEKHIM") 发明人 EROFEEV VLADIMIR IVANOVICH;ERMIZIN KONSTANTIN VLADIMIROVICH;KUZNETSOV NIKOLAJ NIKOLAEVICH;MASKAEV GENNADIJ PAVLOVICH;KOVAL' LJUBOV' MIKHAJLOVNA
分类号 C10G9/14 主分类号 C10G9/14
代理机构 代理人
主权项
地址