<p><P>PROBLEM TO BE SOLVED: To provide a method for producing an inorganic molded body where, when an inorganic molded body is produced by molding a cement based molding material composed of a cement-containing inverse emulsion composition including cement, water and a styrene monomer, and maturing and curing the same, the remaining quantity of the styrene monomer can be efficiently reduced. <P>SOLUTION: A molded body obtained by molding a cement based molding material composed of a cement-containing inverse emulsion composition including cement, water, a styrene monomer and an emulsifying agent is heated at 80 to 100°C, is matured and cured, and is subsequently heated at 110 to 140°C. The polymerization of the styrene monomer can be promoted by the heating after the maturing and curing of the molded body, and the remaining quantity of the styrene monomer in the inorganic molded body can be reduced. <P>COPYRIGHT: (C)2008,JPO&INPIT</p> |